Near-Surface Analysis of Semicondutor Using Grazing Incidence X-Ray Fluorescence

Published online by Cambridge University Press:  06 March 2019

Atsuo Iida
Affiliation:
Photon Factory, National Laboratory for High Energy Physics, Ohomachi, Tsukubagun, Ibarakiken 305, Japan
Kenji Sakurai
Affiliation:
Department of Industrial Chemistry, University of Tokyo Bunkyoku, Tokyo 113, Japan
Yohichi Gohshi
Affiliation:
Department of Industrial Chemistry, University of Tokyo Bunkyoku, Tokyo 113, Japan
Get access

Summary

The X-ray external total reflection was used for the x-ray fluorescence analysis of the near surface layer of a GaAs wafer and a GaAlAs epilayer. Synchrotron radiation was used as an excitation source. The intensity ratio between the Ga K and As K fluorescence signals was measured as a function of the glancing angle. The reduction of As atoms near the surface of less than a hundred Å was observed for the high temperature annealed GaAlAs epilayer.

Information

Type
VIII. Synchrotron Radiation and Other Applications of XRF
Copyright
Copyright © International Centre for Diffraction Data 1987

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

1. Huang, T.C. and Parrish, W., Characterization of Thin Films by X-Ray Fluorescence and Diffraction Analysis, Adv. in X-Ray Anal. 22: 43 (1979)Google Scholar
2. It. Aiginger and Wobrauschek, P., Total reflectance X-Ray Spectrom.try, Adv. in X-Ray Anal. 28: 1 (1985)Google Scholar
3. lida, A., Yoshinaga, A., Salturai, K. and Gohshi, Y., Synchrotron Radiation Excited X-ray Fluorescence Analysis Using Total Reflection of X-Rays, Anal, Chem. 58: 394 (1986)Google Scholar
4. Eichinger, P., Characterization and Analysis of Detector Materials and Processes, Nucl. Instr. and Methods A253: 313 (1987)Google Scholar
5. lida, A., Sakurai, K., A.Yoshinaga and Gohshi, Y., Grazing Incidence X-Ray Fluorescence Analysis, Nucl. Instr. and Methods A246: 736 (1986)Google Scholar
6. Bloch, J.M., Sansone, M., Rondelez, F., Peiffer, D.G., Pincus, P., Kim, M.W. and Eiaenberger, P.M., Concentration Profile of a Dissolved Polymer near the Air-Liquid Interface: X-Ray Fluorescence Study, Phy. Rev. Lett. 54: 1039 (1985)Google Scholar
7. Usami, K., Mochizuki, Y., Minagawa, T., Iida, A. and Gohshi, Y., X-ray Fluorescence Analysis ofHg in SiO2 Filins Deposited by Hg- Sensitized Fhoto-C.D. Jpn. J. Appl. Phys. 25: 1449 (1986)Google Scholar
8. Haieh, J.J., Liquid-Phase Epitaxy, in “Handbook op Semiconductors”, volume 3, Keller, S.P. ed., North-Hoiland (1980)Google Scholar
9. Kudo, H., Ochiai, Y., Takita, K., Masuda, K. and Seki, S., Stoichiometry Measurements of GaAs by Means of 15-MeV He++ Backscattering, J. Appl. Phys. 50: 5034 (1979)Google Scholar
10. Tertian, R. and Claisse, F., “Principles of Quantitative X-Ray Fluorescence Analysis,” Heyden (1982)Google Scholar