Hostname: page-component-857557d7f7-h6shg Total loading time: 0 Render date: 2025-11-21T00:47:45.234Z Has data issue: false hasContentIssue false

Determination of Lattice Parameter and Strain of ϒ' Phases in Nickel-Base Superalloys by Synchrotron Radiation Parallel Beam Diffractometry

Published online by Cambridge University Press:  06 March 2019

Katsumi Ohno
Affiliation:
National Research Institute for Metals 2-3-12 Nakameguro, Meguro-ku Tokyo 153, Japan National Laboratory of High Energy Physics 1-1 Oho Tsukuba-shi Ibaragi-ken 305, Japan
Kazumasa Ohsumi
Affiliation:
National Research Institute for Metals 2-3-12 Nakameguro, Meguro-ku Tokyo 153, Japan National Laboratory of High Energy Physics 1-1 Oho Tsukuba-shi Ibaragi-ken 305, Japan
Hiroshi Harada
Affiliation:
National Research Institute for Metals 2-3-12 Nakameguro, Meguro-ku Tokyo 153, Japan National Laboratory of High Energy Physics 1-1 Oho Tsukuba-shi Ibaragi-ken 305, Japan
Toshihiro Yamagata
Affiliation:
National Research Institute for Metals 2-3-12 Nakameguro, Meguro-ku Tokyo 153, Japan National Laboratory of High Energy Physics 1-1 Oho Tsukuba-shi Ibaragi-ken 305, Japan
Michio Tamazaki
Affiliation:
National Research Institute for Metals 2-3-12 Nakameguro, Meguro-ku Tokyo 153, Japan National Laboratory of High Energy Physics 1-1 Oho Tsukuba-shi Ibaragi-ken 305, Japan
Get access

Abstract

The lattice parameters and strain of ϒ'-phase particles in Nickel-base superalloys, which are duplex type alloys designed for turbine blades and widely called “Ni-base single crystal superalloys”; they are accurately determined by Synchrotron Radiation parallel-beam diffractometry. The superalloys have ϒ' precipitates, an ordered FCC structure based on Ni3Al, in a γ-matrix having disordered FCC structure.

In addition, the preparation method of stress-free ϒ'-phase particles, with no composition change in the preparation process, was newly developed to measure the coherency strain of ϒ'-particles due to lattice misfit. The prepared ϒ'-phase particles are similar in composition and form to ϒ'-phase particles in the γ-matrices. The method for determining of the lattice misfit between the γ and γ’ particles was previously reported.

Information

Type
X. Crystallite Size/Strain Analysis
Copyright
Copyright © International Centre for Diffraction Data 1990

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Article purchase

Temporarily unavailable

References

1. Harada, H., Ohno, K., Yamagata, T., Yokokawa, T. and Yamazaki, M., Superalloys 88, p. 733, (1988).Google Scholar
2. Ohno, K. and Yamazaki, M., Adv. X-Ray Anal., 30:67, (1987).Google Scholar
3. Ohno, K., Harada, H., Yamagata, T. and Yamazaki, M., Tran. ISIJ, 28:218, (1988).10.2355/isijinternational1966.28.218Google Scholar
4. Ohno, K., Harada, H., Yamagata, T. and Yamazaki, M., Adv. X-Ray Anal., 32:365375, (1989).Google Scholar
5. Ohno, K., Fujiwara, J. and Morimoto, I., X-Ray Spectrom., 9:138142, (1980).Google Scholar
6. Klug, H. P. and Alexander, L. E., “X-Ray Diffraction Procedures for Polyerystalline and Amorphous Meterials,” P.755, (1974), John Wily.Google Scholar