5 - Imaging surfaces in TEM

Published online by Cambridge University Press:  18 January 2010

Zhong Lin Wang
Affiliation:
Georgia Institute of Technology
Get access

Summary

Techniques for studying surfaces in TEM

There are two basic modes of TEM operation, namely the bright-field mode, wherein the (000) transmitted beam contributes to the image, and the dark-field imaging mode, in which the (000) beam is excluded. The size of objective aperture in bright-field mode directly determines the information to be emphasized in the final image. When the size is chosen so as to exclude the diffracted beams, one has the configuration that is normally used for low-resolution defect studies, the so-called diffraction contrast. In this case, a crystalline specimen is oriented to excite a particular diffracted beam, or systematic row of reflections. This imaging mode is sensitive to the differences in specimen thickness, distortion of crystal lattices due to defects, strain and bends. High-resolution imaging is usually performed in bright-field mode by including a few Bragg-diffracted beams within the objective aperture. The lattice images are the result of interference between Bragg reflected beams, the so-called phase contrast. In this section, we outline a few techniques that have been extensively developed for studying surfaces in high-resolution TEM (HRTEM) (Cowley, 1986; Smith, 1987).

Imaging using surface-layer reflections

The dark-field imaging technique is favorable for imaging surfaces when the surface layers have different periodicity from that of the bulk of the crystal (Figure 5.1 (a)). Then ‘superlattice’ satellite reflections appear in the diffraction pattern and dark-field imaging with these spots can give high-contrast images of surface structure.

There are two basic mechanisms for generating the superlattice reflections. A sharp termination of the crystal bulk at the surface may form a stacking sequence that is not a complete unit cell.

Information

Type
Chapter
Information
Publisher: Cambridge University Press
Print publication year: 1996

Access options

Get access to the full version of this content by using one of the access options below. (Log in options will check for institutional or personal access. Content may require purchase if you do not have access.)

Book purchase

Temporarily unavailable

Accessibility standard: Unknown

Why this information is here

This section outlines the accessibility features of this content - including support for screen readers, full keyboard navigation and high-contrast display options. This may not be relevant for you.

Accessibility Information

Accessibility compliance for the PDF of this book is currently unknown and may be updated in the future.

Save book to Kindle

To save this book to your Kindle, first ensure no-reply@cambridge.org is added to your Approved Personal Document E-mail List under your Personal Document Settings on the Manage Your Content and Devices page of your Amazon account. Then enter the ‘name’ part of your Kindle email address below. Find out more about saving to your Kindle.

Note you can select to save to either the @free.kindle.com or @kindle.com variations. ‘@free.kindle.com’ emails are free but can only be saved to your device when it is connected to wi-fi. ‘@kindle.com’ emails can be delivered even when you are not connected to wi-fi, but note that service fees apply.

Find out more about the Kindle Personal Document Service.

  • Imaging surfaces in TEM
  • Zhong Lin Wang, Georgia Institute of Technology
  • Book: Reflection Electron Microscopy and Spectroscopy for Surface Analysis
  • Online publication: 18 January 2010
  • Chapter DOI: https://doi.org/10.1017/CBO9780511525254.007
Available formats
×

Save book to Dropbox

To save content items to your account, please confirm that you agree to abide by our usage policies. If this is the first time you use this feature, you will be asked to authorise Cambridge Core to connect with your account. Find out more about saving content to Dropbox.

  • Imaging surfaces in TEM
  • Zhong Lin Wang, Georgia Institute of Technology
  • Book: Reflection Electron Microscopy and Spectroscopy for Surface Analysis
  • Online publication: 18 January 2010
  • Chapter DOI: https://doi.org/10.1017/CBO9780511525254.007
Available formats
×

Save book to Google Drive

To save content items to your account, please confirm that you agree to abide by our usage policies. If this is the first time you use this feature, you will be asked to authorise Cambridge Core to connect with your account. Find out more about saving content to Google Drive.

  • Imaging surfaces in TEM
  • Zhong Lin Wang, Georgia Institute of Technology
  • Book: Reflection Electron Microscopy and Spectroscopy for Surface Analysis
  • Online publication: 18 January 2010
  • Chapter DOI: https://doi.org/10.1017/CBO9780511525254.007
Available formats
×